Home 中文
SEAMLESS AND WELDED AUSTENITIC STAINLESS STEEL SANITARY TUBING
Standard: ASTM A270    
Material: 304, 304L, 316, 316L
OD: 15.9~168.3mm
WT: 0.89, 0.90, 1.00, 1.07, 1.20, 1.24, 1.50, 1.60, 1.65, 2.00, 2.11, 2.77, 3.05mm
Welding method: TIG or TIG + Plasma
Heat Treatment: 1040°C Water Quenching
Stencil: VASTAR, A 270, Grade, OD WT Length, Heat number, Surface finish.
Inspection items: Chemical Composition; Size; Reverse Flattening Test; Hydrostatic Test or Eddy current test; Surface quality; etc.
Application: Food & Dairy industry.

Size Tolerance

 

ASTM

A270 Tolerance

OD Tolerance

WT Tolerance

Length Tolerance

OD

Tolerance

 

OD

Tolerance

25.4mm

±0.13mm

±12.5%

101.6mm

+3.2mm-0mm

>25.4mm, 50.8mm

±0.20mm

>101.6mm

+4.8mm-0mm

>50.8mm,76.2mm

±0.25mm

 

 

>76.2mm,101.6mm

±0.38mm

 

 

>101.6mm,<139.7mm

±0.38mm

 

 

>139.7mm,203.2mm

±0.76mm

 

 

>203.2mm,<304.8mm

±1.27mm

 

 

 

Chemical Composition

ASTM A270  Chemical Composition %

Grade

C

Si

Mn

P

S

Ni

Cr

Mo

304

0.08

1.00

2.00

0.045

0.03

8.00~11.00

18.00~20.00

 

304L

0.035

1.00

2.00

0.045

0.03

8.00~11.00

18.00~20.00

 

316

0.08

1.00

2.00

0.045

0.03

10.00~14.00

16.00~18.00

2.00~3.00

316L

0.035

1.00

2.00

0.045

0.03

10.00~15.00

16.00~18.00

2.00~3.00